Physical Properties Metric English Comments
Bulk Density 0.820 g/cc
0.0296 lb/in³
ASTM D1895
Eastman GP800 PET  (discontinued **)
Voridian PET GP800 is a general purpose polymer that is available in the European, Middle East and Africa region. This product is developed for optimal production of PET bottles, containers, and fil..
Bulk Density 0.820 g/cc
0.0296 lb/in³
ASTM D4894
3M Dyneon™ TR 1105 PTFE  (discontinued **)
Ideal for thin wall ram extrusion productsReduces cold flow and melt viscosityLower permeabilityLower porosityWeldableExcellent product smoothnessIncreased machine outputInformation provided by Dyne..
Bulk Density 0.820 g/cc
0.0296 lb/in³
ISO 60
FKuR Kunststoff Bio-Flex® A 4100 CL Compostable PLA Blend
The BIO-FLEX® trade name indicates blends of co-polyester and PLA* with, depending on the particular grade, a very high content of natural resource material. BIO-FLEX® does not contain any sta..
Bulk Density 0.820 - 0.900 g/cc
0.0296 - 0.0325 lb/in³
SK Chemicals SKYPET® BB7755 Specially Formulated PET Resin
Description: SKYPET-BB7755 is a specially formulated PET resin for PET bottles especially for hot-fill application. SKYPET-BB7755 provides excellent processability in injection molding and blow mol..
Bulk Density 0.820 - 0.900 g/cc
0.0296 - 0.0325 lb/in³
SK Chemicals SKYPET® BL8050 Specially Formulated PET Copolymer Resin
SKYPET-BL8050 is a specially formulated PET copolymer resin for PET bottles and extruded sheet. SKYPET-BL8050 provides excellent processability in injection molding and blow molding processes, offe..
Bulk Density 0.820 - 0.900 g/cc
0.0296 - 0.0325 lb/in³
SK Chemicals SKYPET® BR8040 Low Content CHDM Modified Copolyester Resin
Description: SKYPET-BR8040 is a low content CHDM modified copolyester resin for large sized-mineral water bottles and extruded sheet. SKYPET-BR8040 has sufficiently low crystallization rate for lar..
Bulk Density 0.820 - 0.900 g/cc
0.0296 - 0.0325 lb/in³
SK Chemicals SKYPET® XT8050 Specially Formulated PET Copolymer Resin
Description: SKYPET-XT8050 is a fast reheat grade of SKYPET, specially formulated for high productivity in the blowing process. SKYPET-XT8050 provides excellent processability in injection molding ..
Bulk Density 0.820 - 0.900 g/cc
0.0296 - 0.0325 lb/in³
SK Chemicals SKYPET® BB8055 Specially Formulated PET Resin
Description: SKYPET-BB8055 is a specially formulated PET resin for PET bottles especially for hot-fill application. SKYPET-BB8055 provides excellent processability in injection molding and blow mol..
Bulk Density 0.820 - 0.900 g/cc
0.0296 - 0.0325 lb/in³
SK Chemicals SKYPET® BL8450 Specially Formulated PET Copolymer Resin
Description: SKYPET-BL8450 is a specially formulated PET copolymer resin for PET bottles and extruded sheet. SKYPET-BL8450 provides excellent processability in injection molding and blow molding pr..
Bulk Density 0.820 g/cc
0.0296 lb/in³
ASTM D1895
Plenco 1501 Polyester, Pellet, Injection Molded
PLENCO 01501 is a general purpose, mineral filled granular polyester molding compound, offering excellent arc and track resistance properties, low post shrinkage, and improved mechanical strength va..
Bulk Density 0.820 g/cc
0.0296 lb/in³
Tap
TIMCAL TIMREX® 50X80 mesh Natural Flake Graphite
TIMREX Natural Flake Graphite is produced in a wide range of products distinguished by particle size distribution, chemistry and carbon content. Timcal mines the graphite from its own source in Lac-..
Bulk Density 0.820 g/cc
0.0296 lb/in³
DuPont™ Nomex® N196 Paper, 10 mil Nominal Thickness
Nomex® Type N196 is a high floc grade of Nomex® paper. This leads to a high degree of saturability combined with high stiffness and mechanical properties. Type N196 is used where good saturabili..
Bulk Density 0.820 g/cc
0.0296 lb/in³
DuPont™ Nomex® N196 Paper, 7 mil Nominal Thickness
Nomex® Type N196 is a high floc grade of Nomex® paper. This leads to a high degree of saturability combined with high stiffness and mechanical properties. Type N196 is used where good saturabili..
Bulk Density 0.820 g/cc
0.0296 lb/in³
Asahi Glass Fluon® G340 PTFE Granular Powder
Fluon®PTFE granular powders (molding powders) are used for the production of sheets, rods, billets and other general moldings.Information provided by Asahi Glass Company, Inc.