Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.120 g/cc | 0.00434 lb/in³ | |
Potters Industries Q-Cel® 300 Performance Benefits: A low-density, performance-enhancing additive.Fewer defects: excellent mold flow, uniform dispersionReduced compound density and viscosityIncreased acoustic and thermal insulat.. |
|||
Bulk Density | 0.120 g/cc | 0.00434 lb/in³ | of Dry Beads |
Mo-Sci Corporation GL-0193 Hollow Glass Spheres Appearance: Hollow microspheres with white color in powder form.Applications: GL-0193 is a new, low cost, light weight, hollow glass extender for liquid resin systems offering low cost per unit volu.. |
|||
Bulk Density | 0.120 g/cc | 0.00434 lb/in³ | Tap Density |
Momentive Performance Materials NX1 Boron Nitride (BN) Powder Grades NX1, NX5, NX9, and NX10. The NX line makes BN accessible to users of alternate materials, such as aluminum nitride, alumina, and fused silica, who may have previously ruled out BN.NX grades a.. |
|||
Bulk Density | 0.120 g/cc | 0.00434 lb/in³ | Scott |
TIMCAL TIMREX® MB44 Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |
|||
Bulk Density | 0.120 g/cc | 0.00434 lb/in³ | |
Zircar Zirconia ZYBF-1 Zirconia Bulk Fiber Insulation Zirconia Bulk Fibers Type ZYBF are yttria stabilized zirconia fibers available in five different forms, all having useful properties up to 2200°C. These polycrystalline fibers can be vacuum formed .. |
|||
Bulk Density | 0.120 g/cc | 0.00434 lb/in³ | |
Sinotek Materials Graphite Felt Heat Insulation Material Information provided by Sinotek |
|||
Bulk Density | 0.120 g/cc | 0.00434 lb/in³ | |
Zircar Zirconia ZYBF-1 Zirconia Bulk Fiber Insulation Zirconia Bulk Fibers Type ZYBF are yttria stabilized zirconia fibers available in five different forms, all having useful properties up to 2200°C. These polycrystalline fibers can be vacuum formed .. |