Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 2.95 g/cc | 0.107 lb/in³ | |
Poco Graphite SUPERSiC® Si-3C Silicon Carbide SUPERSiC that has been infiltrated with silicon and then coated with a 75 µm CVD SiC coating, sealing off the porosity.Uses: Ideal for high-temperature vacuum CVD systemsInformation provided by Poc.. |
|||
Bulk Density | 2.95 g/cc | 0.107 lb/in³ | |
Chosun Refractories AMC-65 Alumina Magnesia Carbon Bricks for Ladle Wall And Bottom Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 2.95 g/cc | 0.107 lb/in³ | |
Chosun Refractories ASC-1 Alumina Silicon Carbide Carbon Bricks for Torpedo Car Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 2.96 g/cc | 0.107 lb/in³ | |
Chosun Refractories C15A Magnesia Carbon Brick for Converter Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 2.95 - 3.10 g/cc | 0.107 - 0.112 lb/in³ | |
Chosun Refractories CSN-309NM,Body Plate Brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 2.95 g/cc | 0.107 lb/in³ | |
Chosun Refractories L15H Magnesia Carbon Bricks for Ladle Slag Line Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 2.95 g/cc | 0.107 lb/in³ | |
Chosun Refractories L15HU Magnesia Carbon Bricks for Ladle Slag Line Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 2.95 g/cc | 0.107 lb/in³ | |
Chosun Refractories L15S Magnesia Carbon Bricks for Ladle Slag Line Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 2.95 g/cc | 0.107 lb/in³ | |
Chosun Refractories SAL85 Special Alumina brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | >= 2.95 g/cc | >= 0.107 lb/in³ | |
China-Yixing Longly Refractories Shelf Corundum-Mullite Products with high-purity fused alumina and fused mullite for raw materials, the use of high-tonnage press repression, from ultra-high-temperature sintering; high-purity, the main phase (or corundum.. |
|||
Bulk Density | 2.95 g/cc | 0.107 lb/in³ | |
Poco Graphite SUPERSiC® Si-8C Silicon Carbide SUPERSiC that has been infiltrated with silicon and then coated with a 200 µm CVD SiC coatingUses: Ideal for optical and lithography componentsInformation provided by Poco Graphite |