Physical Properties Metric English Comments
Bulk Density 2.55 - 2.65 g/cc
0.0921 - 0.0957 lb/in³
After drying at 110°C
Gouda Vuurvast CURON 150 RN Dense Refractory Castable
Description: This on sintered bauxite and low-iron alumina cement based castable contains stainless steel fibers, what results in a very good mechanical strength.Remarks: These values apply to cast ..
Bulk Density 2.55 - 2.65 g/cc
0.0921 - 0.0957 lb/in³
After drying at 110°C
Gouda Vuurvast CURON 170 GM Dense Refractory Castable
Description: A general purpose gunning castable with a wide range of applications for high temperatures. The low Fe2O3 content makes this castable suitable for use under reducing conditions.Remarks:..
Bulk Density 2.55 - 2.65 g/cc
0.0921 - 0.0957 lb/in³
After drying at 110°C
Gouda Vuurvast CURON 180 T SP GM Dense Refractory Castable
Description: Curon 180 T SP GM is a gunning castable based on tabular alumina for application at very high temperatures.Remarks: These values apply to cast products.Information provided by Gouda Vuu..
Bulk Density 2.55 - 2.65 g/cc
0.0921 - 0.0957 lb/in³
After drying at 110°C
Gouda Vuurvast FLUCON 160 H SiC (R) Dense Self Flowing Refractory Castable
Description: Flucon 160 H SiC (R) is a self-flowing low cement castable, characterized by a high strength and good slag resistance. Because of the presence of SiC this material has a very good resis..
Bulk Density 2.55 - 2.65 g/cc
0.0921 - 0.0957 lb/in³
After drying at 110°C
Gouda Vuurvast VIBRON 160 H GS (R) Dense Vibrating Refractory Castable
Description: Vibron 160 H GS (R) is a pumpable low cement castable based on high fired high alumina grog and characterized by a high strength and good thermal shock-, corrosion- and abrasion resista..
Bulk Density 2.55 - 2.65 g/cc
0.0921 - 0.0957 lb/in³
After drying at 110°C
Gouda Vuurvast VIBRON 160 K Dense Vibrating Refractory Castable
Description: Vibron 160 K is a low cement castable based on silicon carbide and characterized by a very good thermal conductivity and high abrasion resistance. The thermal shock resistance is excell..
Bulk Density 2.60 - 2.65 g/cc
0.0939 - 0.0957 lb/in³
China-Yixing Longly Refractories Seggar SiC
SiC series products of SiC shelf boards, SiC pillars, SiC slab, SiC seggar kiln furniture, are formed using high-quality silicon carbide materials and high temperature binders by tons of high-vibrat..