Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 2.45 - 2.55 g/cc | 0.0885 - 0.0921 lb/in³ | After drying at 110°C |
Gouda Vuurvast CURON 160 Dense Refractory Castable Description: Because of the selection of raw materials this castable has a high volume stability and maintains its strength up to high temperatures. In addition Curon 160 has an excellent thermal sh.. |
|||
Bulk Density | 2.45 - 2.55 g/cc | 0.0885 - 0.0921 lb/in³ | After drying at 110°C |
Gouda Vuurvast CURON 180 L Dense Refractory Castable Description: Curon 180 L is a castable based on fused alumina for use up to 1800°C and shows a good thermal shock resistance.Remarks: These values apply to cast products. Also available in gunnin.. |
|||
Bulk Density | 2.45 - 2.55 g/cc | 0.0885 - 0.0921 lb/in³ | After drying at 110°C |
Gouda Vuurvast VIBRON 160 H Dense Vibrating Refractory Castable Description: Vibron 160 H is a low cement castable based on high fired high alumina grog and characterized by a high strength and good thermal shock resistance.Remarks: Indicated values apply to vib.. |
|||
Bulk Density | 2.45 - 2.55 g/cc | 0.0885 - 0.0921 lb/in³ | After drying at 110°C |
Gouda Vuurvast VIBRON 160 H SiC Dense Vibrating Refractory Castable Description: Vibron 160 H SiC is a low cement vibrating castable characterized by a high strength, good abrasion resistance and excellent thermal shock resistance. Because of the presence of SiC, th.. |
|||
Bulk Density | 2.45 g/cc | 0.0885 lb/in³ | |
Chosun Refractories CRAG-S27 Long Stopper Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 2.45 g/cc | 0.0885 lb/in³ | |
Chosun Refractories SBSN20 Nozzle Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 2.45 g/cc | 0.0885 lb/in³ | |
Chosun Refractories TD-165H Special Casting Block Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |