Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 1.26 g/cc | 0.0454 lb/in³ | Powder |
Aremco Ceramacast™ 675-N High Temperature Potting & Casting Material Aluminum Nitride Fine grain aluminum nitride castable with high thermal conductivity. |