Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.0350 g/cc | 0.00126 lb/in³ | |
Zircar Zirconia Buster Mat Alumina Insulation Buster Blanket and Buster Mat are flexible, Hi-Alpha alumina fiber insulation materials. The mat is 100% fibers while the blanket has been needled into a durable blanket with the addition of an orga.. |
|||
Bulk Density | 0.0350 g/cc | 0.00126 lb/in³ | Minimum |
SYNTHOS Koplen® 0207 FR Expandable Polystyrene Low Pentane Self-Extinguishing type Koplen®.Processing Method: By water steam or hot water, the volume of the beads is increased. Foam-processing to thin-wall moldings. Lower density can be achie.. |
|||
Bulk Density | 0.0350 g/cc | 0.00126 lb/in³ | |
Zircar Refractory Composites RSMAT-3000 ALUMINA MAT ZRCI Type RSMAT-3000 is a high purity, high temperature, flexible form composed of continuous 97% alumina ceramic fibers designed for use to 1650°C (3002°F). Type RSMAT-3000 contains little shot a.. |
|||
Bulk Density | 0.0350 g/cc | 0.00126 lb/in³ | |
Zircar Zirconia Buster Mat Alumina Insulation Buster Blanket and Buster Mat are flexible, Hi-Alpha alumina fiber insulation materials. The mat is 100% fibers while the blanket has been needled into a durable blanket with the addition of an orga.. |