SYNTHOS Koplen® 0207 FR Expandable Polystyrene

Category Polymer , Thermoplastic , Polystyrene (PS) , Expanded Polystyrene (EPS)
Manufacturer SYNTHOS Kralupy a.s.
Trade Name Koplen®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SYNTHOS Koplen® 0207 FR Expandable Polystyrene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Low Pentane Self-Extinguishing type Koplen®.Processing Method: By water steam or hot water, the volume of the beads is increased. Foam-processing to thin-wall moldings. Lower density can be achieved after several preforming operations.Typical Application: Thin walled products with walls under 10mm. Light weight ceramics, light weight wall plaster and concrete mix. False ceilings.Synthos was formerly known as Kaucuk. All information provided by Synthos.
Physical Properties Metric English Comments
Bulk Density >= 0.0250 g/cc
>= 0.000903 lb/in³
Typical
0.0350 g/cc
0.00126 lb/in³
Minimum
Particle Size 400 - 630 µm
400 - 630 µm