Polymer Property : Bulk Density = 0.0298 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Bulk Density 0.826 g/cc
0.0298 lb/in³
Poured; ASTM D1895
Eastman Aqua WA314 PET  (discontinued **)
Voridian Aqua PET WA314 is a polyethylene terephthalate resin designed for single-serve bottled water applications. WA314 has an intrinsic viscosity of 0.76 and provides sparkling clarity and fast i..