Eastman Aqua WA314 PET  (discontinued **)

Category Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET) , Polyethylene Terephthalate (PET), Unreinforced
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Eastman Aqua WA314 PET  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Voridian Aqua PET WA314 is a polyethylene terephthalate resin designed for single-serve bottled water applications. WA314 has an intrinsic viscosity of 0.76 and provides sparkling clarity and fast injection molding cycles.Applications/UsesWater bottlesKey AttributesFast injection molding cyclesSparkling clarity
Physical Properties Metric English Comments
Bulk Density 0.826 g/cc
0.0298 lb/in³
Poured; ASTM D1895
0.894 g/cc
0.0323 lb/in³
Vibrated; ASTM D1895
Melt Density 1.10 g/cc

@Temperature 285 °C
0.0397 lb/in³

@Temperature 545 °F
ASTM D1238
Viscosity Measurement 0.74 - 0.78
0.74 - 0.78
Intrinsic; VGAS-A-AN-G-V-1
Thermal Properties Metric English Comments
Melting Point 243 °C
469 °F
Crystalline Peak Melting Point; ASTM D3418
Descriptive Properties Value Comments
Acetaldehyde <1ppm
VKCA-A-AS-G-GC-0001
Color, CIE L* 80.3 min
VGAS-A-AN-G-RS-001
Fines, wt%, max 0.1