Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Bulk Density = 0.0173 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Bulk Density 0.320 - 0.480 g/cc
0.0116 - 0.0173 lb/in³
Protective Coating PC-Wood Guardian™ Wood Preservative
PC-Wood Guardian™ isused in preventing and controlling decay fungi. It is an effective treatment for wood and wood composite to kill and prevent infestations of decay fungi including white and brow..
Bulk Density 0.400 - 0.480 g/cc
0.0145 - 0.0173 lb/in³
Trelleborg Fillite® 160W Alumino-silicate Cenospheres
Fillite is a glass hard, inert, hollow silicate sphere. Fillite is primarily used to reduce the weight of plastics, rubbers, resins, cement, etc., but also imparts further benefits in many situatio..
Bulk Density 0.400 - 0.480 g/cc
0.0145 - 0.0173 lb/in³
Trelleborg Fillite® SGHA (500HA) Alumino-silicate Cenospheres
Fillite is a glass hard, inert, hollow silicate sphere. Fillite is primarily used to reduce the weight of plastics, rubbers, resins, cement, etc., but also imparts further benefits in many situatio..
Bulk Density 0.400 - 0.480 g/cc
0.0145 - 0.0173 lb/in³
Trelleborg Fillite® 300W Alumino-silicate Cenospheres
Fillite is a glass hard, inert, hollow silicate sphere. Fillite is primarily used to reduce the weight of plastics, rubbers, resins, cement, etc., but also imparts further benefits in many situatio..
Bulk Density 0.400 - 0.480 g/cc
0.0145 - 0.0173 lb/in³
Dried
Zircar Ceramics SALI Moldable Alumina Insulation
A close cousin to premium grade Type SALI insulation, SALI Moldable is a thick doughy material readily shaped into complex forms using molds & hand building techniques or applied to surfaces. When ..
Bulk Density 0.380 - 0.480 g/cc
0.0137 - 0.0173 lb/in³
Tap; ASTM D4164
CRP Technology Windform® PS Polystyrene for Selective Laser Sintering
Windform® PS is a polystyrene based material, developed specifically to produce complex investment casting patterns. The sintered patterns are ideal for conventional wax infiltration, and become ea..
Bulk Density 0.400 - 0.480 g/cc
0.0145 - 0.0173 lb/in³
Akzo Nobel Expancel® 092 MB 120 Masterbatch with unexpanded microspheres
Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the..