Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Zircar Ceramics SALI Moldable Alumina Insulation

Category Ceramic , Oxide , Aluminum Oxide
Manufacturer Zircar Ceramics
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Zircar Ceramics SALI Moldable Alumina Insulation.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A close cousin to premium grade Type SALI insulation, SALI Moldable is a thick doughy material readily shaped into complex forms using molds & hand building techniques or applied to surfaces. When dried and fired, parts made of it are useful to 1700°C (3092°F). Information provided by Zircar Ceramics.
Physical Properties Metric English Comments
Bulk Density 0.400 - 0.480 g/cc
0.0145 - 0.0173 lb/in³
Dried
Density 0.960 g/cc
0.0347 lb/in³
Placing Density
Solids Content >= 42 %
>= 42 %
pH 6.5 - 7.0
6.5 - 7.0
Thermal Properties Metric English Comments
Melting Point 1927 °C
3501 °F
Maximum Service Temperature, Air 1700 °C
3090 °F
Shrinkage <= 20 %
<= 20 %
Drying: Volume
<= 3.00 %

@Temperature 1700 °C,
Time 86400 sec
<= 3.00 %

@Temperature 3090 °F,
Time 24.0 hour
Perpendicular to Thickness
Component Elements Properties Metric English Comments
Al2O3 80 %
80 %
Na2O <= 0.10 %
<= 0.10 %
SiO2 20 %
20 %
Descriptive Properties Value Comments
Color White