Polymer Property : Bulk Density = 0.00181 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Bulk Density 0.0500 g/cc
0.00181 lb/in³
After expansion; ASTM D3575
Sekisui PIOCELAN LSP-20D Moldable Polymer Foam
A hybrid moldable resin material PIOCLEAN, consisting of polystyrene and polyolefin, achieves performance exceeding that of the individual components by effectively combining materials with drastica..
Bulk Density 0.0500 g/cc
0.00181 lb/in³
After expansion; ASTM D3575
Sekisui PIOCELAN LSP-20DB Moldable Polymer Foam
A hybrid moldable resin material PIOCLEAN, consisting of polystyrene and polyolefin, achieves performance exceeding that of the individual components by effectively combining materials with drastica..
Bulk Density 0.0500 g/cc
0.00181 lb/in³
After expansion
Sekisui PIOCELAN OP-20D Moldable Polymer Foam
A hybrid moldable resin material PIOCLEAN, consisting of polystyrene and polyolefin, achieves performance exceeding that of the individual components by effectively combining materials with drastica..
Bulk Density 0.0500 g/cc
0.00181 lb/in³
After expansion; ASTM D3575
Sekisui PIOCELAN OP-20DB Moldable Polymer Foam
A hybrid moldable resin material PIOCLEAN, consisting of polystyrene and polyolefin, achieves performance exceeding that of the individual components by effectively combining materials with drastica..
Bulk Density 0.0500 g/cc
0.00181 lb/in³
SPHERE ONE EXTENDOSPHERESâ„¢ PM 6550 Hollow Plastic Spheres
PM 6550 PM 6550 is an extremely light and versatile hollow sphere. Its plastic composition results in a very low density product. Only a very small amount of this hollow sphere is needed to provide ..
Bulk Density 0.0500 g/cc
0.00181 lb/in³
Scott, Typical
TIMCAL TIMREX® PP 10 Natural Flake Graphite
TIMREX Natural Flake Graphite is produced in a wide range of products distinguished by particle size distribution, chemistry and carbon content. Timcal mines the graphite from its own source in Lac-..
Bulk Density 0.0500 - 0.0600 g/cc
0.00181 - 0.00217 lb/in³
BASF Neopolen® P 9255 0.07 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 9255 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9255.Note: In order to mea..
Bulk Density 0.0500 - 0.0600 g/cc
0.00181 - 0.00217 lb/in³
BASF Neopolen® P 9255 0.09 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 9255 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9255.Note: In order to mea..
Bulk Density 0.0500 - 0.0600 g/cc
0.00181 - 0.00217 lb/in³
BASF Neopolen® P 9255 0.06 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 9255 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9255.Note: In order to mea..
Bulk Density 0.0500 - 0.0600 g/cc
0.00181 - 0.00217 lb/in³
BASF Neopolen® P 9255 0.08 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 9255 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9255.Note: In order to mea..