Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.0500 g/cc | 0.00181 lb/in³ | After expansion; ASTM D3575 |
Sekisui PIOCELAN LSP-20D Moldable Polymer Foam A hybrid moldable resin material PIOCLEAN, consisting of polystyrene and polyolefin, achieves performance exceeding that of the individual components by effectively combining materials with drastica.. |
|||
Bulk Density | 0.0500 g/cc | 0.00181 lb/in³ | After expansion; ASTM D3575 |
Sekisui PIOCELAN LSP-20DB Moldable Polymer Foam A hybrid moldable resin material PIOCLEAN, consisting of polystyrene and polyolefin, achieves performance exceeding that of the individual components by effectively combining materials with drastica.. |
|||
Bulk Density | 0.0500 g/cc | 0.00181 lb/in³ | After expansion |
Sekisui PIOCELAN OP-20D Moldable Polymer Foam A hybrid moldable resin material PIOCLEAN, consisting of polystyrene and polyolefin, achieves performance exceeding that of the individual components by effectively combining materials with drastica.. |
|||
Bulk Density | 0.0500 g/cc | 0.00181 lb/in³ | After expansion; ASTM D3575 |
Sekisui PIOCELAN OP-20DB Moldable Polymer Foam A hybrid moldable resin material PIOCLEAN, consisting of polystyrene and polyolefin, achieves performance exceeding that of the individual components by effectively combining materials with drastica.. |
|||
Bulk Density | 0.0500 g/cc | 0.00181 lb/in³ | |
SPHERE ONE EXTENDOSPHERESâ„¢ PM 6550 Hollow Plastic Spheres PM 6550 PM 6550 is an extremely light and versatile hollow sphere. Its plastic composition results in a very low density product. Only a very small amount of this hollow sphere is needed to provide .. |
|||
Bulk Density | 0.0500 g/cc | 0.00181 lb/in³ | Scott, Typical |
TIMCAL TIMREX® PP 10 Natural Flake Graphite TIMREX Natural Flake Graphite is produced in a wide range of products distinguished by particle size distribution, chemistry and carbon content. Timcal mines the graphite from its own source in Lac-.. |
|||
Bulk Density | 0.0500 - 0.0600 g/cc | 0.00181 - 0.00217 lb/in³ | |
BASF Neopolen® P 9255 0.07 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9255 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9255.Note: In order to mea.. |
|||
Bulk Density | 0.0500 - 0.0600 g/cc | 0.00181 - 0.00217 lb/in³ | |
BASF Neopolen® P 9255 0.09 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9255 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9255.Note: In order to mea.. |
|||
Bulk Density | 0.0500 - 0.0600 g/cc | 0.00181 - 0.00217 lb/in³ | |
BASF Neopolen® P 9255 0.06 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9255 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9255.Note: In order to mea.. |
|||
Bulk Density | 0.0500 - 0.0600 g/cc | 0.00181 - 0.00217 lb/in³ | |
BASF Neopolen® P 9255 0.08 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9255 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9255.Note: In order to mea.. |