Physical Properties | Metric | English | Comments |
---|---|---|---|
Spiral Flow | 12.5 cm @Thickness 1.00 mm |
4.92 in @Thickness 0.0394 in |
390°C nozzle, 180°C tool; Victrex |
Victrex® PEEK 650G Polyetheretherketone Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding and extrusion, low viscosity, FDA food conta.. |