Physical Properties Metric English Comments
Spiral Flow 12.5 cm

@Thickness 1.00 mm
4.92 in

@Thickness 0.0394 in
390°C nozzle, 180°C tool; Victrex
Victrex® PEEK 650G Polyetheretherketone
Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding and extrusion, low viscosity, FDA food conta..