Physical Properties Metric English Comments
Spiral Flow 33.0 cm

@Thickness 3.00 mm
13.0 in

@Thickness 0.118 in
395°C nozzle, 200°C tool
Victrex® PEEK 450CA30 30% Carbon Fiber Reinforced
General purpose, 30% carbon fiber reinforced, pelletized grade for injection molding.Information provided by Victrex.
Spiral Flow 33.0 cm

@Thickness 1.00 mm
13.0 in

@Thickness 0.0394 in
400°C nozzle, 200°C tool
Victrex® PEEK 90G Polyetheretherketone, Unreinforced