Physical Properties Metric English Comments
Viscosity Measure 1500 cSt
1500 cSt
kinetic/kinematic
Dow Corning 1503 Fluid
A blend of an ultra high viscosity dimethiconol in a low viscosity dimethicone fluid for use in skincare, woundcare, scar therapy, suncare, and color cosmetic applications.Information provided by Do..