Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity Measure | 13.5 cSt | 13.5 cSt | 5.23% Toluene solution; MA-04-3-003 |
Dynasol Calprene® 405 Thermoplastic Rubber (SBS) Calprene 405 is a 67/33 Butadiene/Styrene thermoplastic copolymer, polymerized in solution. It has a radial structure. This product is presented in porous crumb form, which gives good oil absorption.. |