Dynasol Calprene® 405 Thermoplastic Rubber (SBS)

Category Polymer , Thermoplastic , Elastomer, TPE , Styrenic TPE
Manufacturer Dynasol
Trade Name Calprene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dynasol Calprene® 405 Thermoplastic Rubber (SBS).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Calprene 405 is a 67/33 Butadiene/Styrene thermoplastic copolymer, polymerized in solution. It has a radial structure. This product is presented in porous crumb form, which gives good oil absorption.Applications: FootwearSportswearMechanical rubber goodsBitumen modificationInformation provided by Dynasol.
Physical Properties Metric English Comments
Volatiles <= 0.40 %
<= 0.40 %
ASTM D5668
Viscosity Measure 13.5 cSt
13.5 cSt
5.23% Toluene solution; MA-04-3-003
Ash <= 0.35 %
<= 0.35 %
ASTM D5667
Mechanical Properties Metric English Comments
Hardness, Shore A 86
86
ASTM D2240
Chemical Properties Metric English Comments
Styrene Content 33 %
33 %
on polymer; MA-04-3-062
Descriptive Properties Value Comments
Color 2
Hunterlab, ASTM D1925-70
Insolubles <0.1%
in toluene, 324 mesh, MA 04-3-018