Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity Measure | >= 1.00e+6 cSt @Temperature 40.0 °C |
>= 1.00e+6 cSt @Temperature 104 °F |
Kinematic Viscosity; ASTM D445 |
Donnelly Bros HT 250 High Temperature Mold Grease Off white, smooth appearance. Works well in constant metal temperature of 200° F to 250° F. (Note: The plastic molding material itself might be >600° F.)A stiff, silica thickened, medium viscos.. |
|||
Viscosity Measure | >= 1.00e+6 cSt | >= 1.00e+6 cSt | internal phase |
Dow Corning 1784 EMULSION A 50 percent anionic emulsion of high molecular weight polydimethylsiloxane for use in shower gels and hair care applications.Information provided by Dow Corning |
|||
Viscosity Measure | >= 1.00e+6 cSt | >= 1.00e+6 cSt | internal phase |
Dow Corning 1785 EMULSION A 60 percent anionic emulsion of high molecular weight polydimethylsiloxane for use in shower gels and hair care applications.Information provided by Dow Corning |
|||
Viscosity Measure | >= 1.00e+6 cSt | >= 1.00e+6 cSt | Internal Phase |
Dow Corning XIAMETER® PMCPMEM-1784 Emulsion Is chemically equivalent to DOW CORNING® 1784 EMULSION. A 50 percent anionic emulsion of high molecular weight OH functional polydimethylsiloxane for use in shower gels and hair care applications. .. |