Dow Corning XIAMETER® PMCPMEM-1784 Emulsion

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer Dow Corning
Trade Name XIAMETER®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning XIAMETER® PMCPMEM-1784 Emulsion.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Is chemically equivalent to DOW CORNING® 1784 EMULSION. A 50 percent anionic emulsion of high molecular weight OH functional polydimethylsiloxane for use in shower gels and hair care applications. INCI Name: Dimethiconol (and) TEA-DodecylbenzenesulfonateInformation provided by Dow Corning
Physical Properties Metric English Comments
pH 6.0 - 8.0
6.0 - 8.0
Viscosity Measure >= 20 cSt
>= 20 cSt
Kinetic/Kinematic
>= 1.00e+6 cSt
>= 1.00e+6 cSt
Internal Phase
Descriptive Properties Value Comments
Active Content (%) 50
Anionic Yes