Polymer Property : Linear Mold Shrinkage, Transverse = 0.0317 cm/cm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.0317 cm/cm

@Time 86400 sec
0.0317 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP STAT-KON RD000IXP PA 66
LNP STAT-KON* RD000IXP is a compound based on Nylon 66 resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact.