Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.020 - 0.022 cm/cm @Time 86400 sec |
0.020 - 0.022 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP KL004A Acetal Homopolymer LNP LUBRICOMP* KL004A is a compound based on Acetal Homopolymer resin containing 20% PTFE. Added feature of this material is: Wear Resistant. |
|||
Linear Mold Shrinkage, Transverse | 0.020 - 0.022 cm/cm @Time 86400 sec |
0.020 - 0.022 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP KL004AXC Acetal Homopolymer LNP* LUBRICOMP* KL004AXC is a compound based on Acetal Homopolymer resin containing 20% PTFE. Added feature of this material is: Wear Resistant. |
|||
Linear Mold Shrinkage, Transverse | 0.019 - 0.022 cm/cm @Time 86400 sec |
0.019 - 0.022 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP STAT-KON FX98500 PE LNP* STAT-KON* FX98500 is a compound based on Polyethylene resin containing Proprietary Filler(s). Added feature of this material is: Electrically Conductive. |
|||
Linear Mold Shrinkage, Transverse | 0.019 - 0.022 cm/cm @Time 86400 sec |
0.019 - 0.022 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP STAT-KON FX98500 PE LNP* STAT-KON* FX98500 is a compound based on Polyethylene resin containing Proprietary Filler(s). Added feature of this material is: Electrically Conductive. |
|||
Linear Mold Shrinkage, Transverse | 0.019 - 0.022 cm/cm @Time 86400 sec |
0.019 - 0.022 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP STAT-KON FX98500C PE LNP* STAT-KON* FX98500C is a compound based on Polyethylene resin containing Proprietary Filler(s). Added feature of this material is: Electrically Conductive. |
|||
Linear Mold Shrinkage, Transverse | 0.019 - 0.022 cm/cm @Time 86400 sec |
0.019 - 0.022 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP STAT-KON FX98500C PE LNP* STAT-KON* FX98500C is a compound based on Polyethylene resin containing Proprietary Filler(s). Added feature of this material is: Electrically Conductive. |