Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.0199 cm/cm @Time 86400 sec |
0.0199 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP Stat-loy W3000 PBT LNP STAT-LOY* W3000 is a compound based on Polybutylene Terephalate resin containing Anti-Static. Added features of this material include: Antistat.This data was supplied by SABIC-IP for the Americ.. |