Polymer Property : Linear Mold Shrinkage, Transverse = 0.0079 cm/cm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.0079 cm/cm

@Time 86400 sec
0.0079 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP LUBRICOMP DL002ER PC
LNP* Lubricomp* DL002ER is a compound based on Polycarbonate resin containing 10% PTFE. Added features of this material include: Internally Lubricated, Easy Molding, Mold Release.
Linear Mold Shrinkage, Transverse 0.0079 cm/cm

@Thickness 3.20 mm
0.0079 in/in

@Thickness 0.126 in
3.2x7.6x12.6mm; ASTM D955
Lavergne VYPET VNT 340 PET 40% Glass - Mineral Reinforced
Vypet VNT 340 is a 40% glass/mineral reinforced PET injection molding compound designed for electrical and structural applications, with High Dielectric StrengthFeatures: High temperature performanc..
Linear Mold Shrinkage, Transverse 0.0079 cm/cm

@Time 86400 sec
0.0079 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP LUBRICOMP RX03643H PA 66
LNP* LUBRICOMP* RX03643H is a compound based on Nylon 66 resin containing Proprietary Filler(s). Added feature of this material is: Wear Resistant.
Linear Mold Shrinkage, Transverse 0.0079 cm/cm

@Time 86400 sec
0.0079 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP LUBRICOMP RX03643H PA 66 (Asia Pacific)
LNP* Lubricomp* RX03643H is a compound based on Nylon 66 resin containing Proprietary Filler(s). Added features of this material include: Internally Lubricated.
Linear Mold Shrinkage, Transverse 0.0079 cm/cm

@Time 86400 sec
0.0079 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP STAT-KON DD0009PC PC
LNP STAT-KON* DD0009PC is a compound based on Polycarbonate resin containing Carbon Powder. Added features of this material include: Electrically Conductive, Flame Retardant.
Linear Mold Shrinkage, Transverse 0.0079 cm/cm

@Time 86400 sec
0.0079 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP LUBRICOMP DL002ER PC (Asia Pacific)
LNP* Lubricomp* DL002ER is a compound based on Polycarbonate resin containing PTFE. Added features of this material include: Internally Lubricated, Easy Molding, Mold Release.