Polymer Property : Linear Mold Shrinkage, Transverse = 0.0067 cm/cm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.0067 cm/cm

@Time 86400 sec
0.0067 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP LUBRICOMP DFL32 PC
LNP LUBRICOMP* DFL32 is a compound based on Polycarbonate resin containing 10% Glass Fiber and 15% PTFE. Added features of this material include: Internally Lubricated.
Linear Mold Shrinkage, Transverse 0.0067 cm/cm

@Time 86400 sec
0.0067 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP LUBRICOMP DFL32XXC PC
LNP LUBRICOMP* DFL32XXC is a compound based on Polycarbonate resin containing 10% Glass Fiber, 15% PTFE. Added features of this material include: Internally Lubricated.
Linear Mold Shrinkage, Transverse 0.0067 cm/cm

@Time 86400 sec
0.0067 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP STAT-KON DX93500 PC
LNP STAT-KON* DX93500 is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added feature of this material is: Electrically Conductive.
Linear Mold Shrinkage, Transverse 0.0067 cm/cm

@Time 86400 sec
0.0067 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP STAT-KON REP349 PA 66
LNP* STAT-KON* REP349 is a compound based on Nylon 66 resin containing 15% PTFE/Silicone, 20% Carbon Fiber. Added features of this material include: Electrically Conductive, Wear Resistant.
Linear Mold Shrinkage, Transverse 0.0067 cm/cm

@Time 86400 sec
0.0067 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP STAT-KON REP349 PA 66 (Asia Pacific)
LNP* Stat-kon* REP349 is a compound based on Nylon 66 resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive, Internally Lubricated.
Linear Mold Shrinkage, Transverse 0.0067 cm/cm

@Time 86400 sec
0.0067 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP STAT-KON RX05488 PA 66
LNP STAT-KON* RX05488 is a compound based on Nylon 66 resin containing Carbon Fiber, Flame Retardant, Glass Fiber, PTFE. Added features of this material include: Electrically Conductive.
Linear Mold Shrinkage, Transverse 0.0067 cm/cm

@Time 86400 sec
0.0067 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP THERMOCOMP DF004P PC
LNP THERMOCOMP* DF004P is a compound based on Polycarbonate resin containing 20% Glass Fiber. Added features of this material include: Exceptional Processing.
Linear Mold Shrinkage, Transverse 0.0067 cm/cm

@Time 86400 sec
0.0067 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP THERMOCOMP DF006P PC
LNP THERMOCOMP* DF006P is a compound based on Polycarbonate resin containing 30% Glass Fiber. Added features of this material include: Exceptional Processing.
Linear Mold Shrinkage, Transverse 0.0067 cm/cm

@Time 86400 sec
0.0067 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP THERMOCOMP JF003XXZ PES
LNP* THERMOCOMP* JF003XXZ is a compound based on Polyethersulfone resin containing 15% Glass Fiber.
Linear Mold Shrinkage, Transverse 0.0067 cm/cm

@Time 86400 sec
0.0067 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP THERMOCOMP JF003XXZ PES (Asia Pacific)
LNP* Thermocomp* JF003XXZ is a compound based on Polyethersulfone resin containing Glass Fiber.
Linear Mold Shrinkage, Transverse 0.0067 cm/cm

@Time 86400 sec
0.0067 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP Thermocomp TH0450D
LNP* Thermocomp* TH0450D is a compound based on Polyurethane resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity.This data was supplied by ..
Linear Mold Shrinkage, Transverse 0.0067 cm/cm

@Time 86400 sec
0.0067 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP Thermocomp TH0450D PUR (Asia Pacific)
LNP* Thermocomp* TH0450D is a compound based on Polyurethane resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity.This data was supplied by ..
Linear Mold Shrinkage, Transverse 0.0067 cm/cm

@Time 86400 sec
0.0067 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP THERMOTUF OF006I PPS - Linear
LNP THERMOTUF* OF006I is a compound based on PPS - Linear resin containing Glass Fiber. Added features of this material include: High Impact.