Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.0038 cm/cm @Time 86400 sec |
0.0038 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP STAT-KON DE0039 PC LNP* STAT-KON* DE0039 is a compound based on Polycarbonate resin containing 15% Carbon Fiber. Added features of this material include: Flame Retardant. Electrically Conductive. |
|||
Linear Mold Shrinkage, Transverse | 0.0038 cm/cm @Time 86400 sec |
0.0038 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP THERMOCOMP AF002 ABS LNP THERMOCOMP* AF002 is a compound based on ABS resin containing 10% Glass Fiber. |
|||
Linear Mold Shrinkage, Transverse | 0.0038 cm/cm @Time 86400 sec |
0.0038 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP STAT-KON DE0039 PC (Asia Pacific) LNP* Stat-kon* DE0039 is a compound based on Polycarbonate resin containing Flame Retardant, Carbon Fiber. Added features of this material include: Flame Retardant. |
|||
Linear Mold Shrinkage, Transverse | 0.0038 cm/cm @Time 86400 sec |
0.0038 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP Stat-kon DX96690 PC LNP STAT-KON* DX96690 is a compound based on Polycarbonate resin containing PTFE. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for the America.. |
|||
Linear Mold Shrinkage, Transverse | 0.0038 cm/cm @Time 86400 sec |
0.0038 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP THERMOCOMP AF002XXC ABS LNP THERMOCOMP* AF002XXC is a compound based on ABS resin containing 10% Glass Fiber. |