Physical Properties | Metric | English | Comments |
---|---|---|---|
a Lattice Constant | 3.252 Ã… | 3.252 Ã… | |
MarkeTech Zinc Oxide (ZnO) Single Crystal Substrate Data provided by the supplier, MarkeTech International.Used as a substrate for deposition of high temperature oxide superconductors. |
|||
a Lattice Constant | 3.252 Ã… | 3.252 Ã… | |
Mateck Zinc Oxide, ZnO |