a Lattice Constant 3.252 Ã…
3.252 Ã…
MarkeTech Zinc Oxide (ZnO) Single Crystal Substrate
Data provided by the supplier, MarkeTech International.Used as a substrate for deposition of high temperature oxide superconductors.
a Lattice Constant 3.252 Ã…
3.252 Ã…
Mateck Zinc Oxide, ZnO