Physical Properties Metric English Comments
a Lattice Constant 3.08 Ã…
3.08 Ã…
MarkeTech Silicon Carbide (6H) Single Crystal Substrate
Data provided by the supplier, MarkeTech International.Developed for deposition of III-V nitrides for LEDs, Lasers, etc. Standard orientation: ; GaN Lattice Mismatch 3.5%.
a Lattice Constant 3.08 Å
3.08 Å
Mateck Silicon Carbide Substrate, SiC (6H)
Substrate single crystals for III-V nitrides