Physical Properties | Metric | English | Comments |
---|---|---|---|
Coating Weight | 46.6 g/m² | 29.1 lb/ream | ExxonMobil Method |
ExxonMobil Bicor™ 52MBR666 OPP Film Product Description: Bicor 52MBR666 is a biaxially oriented transparent polypropylene film coated with humidity resistant acrylic on both sides. This film is designed to wrap products with a high mo.. |