Polymer Property : Coating Weight = 29.1 lb/ream Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Coating Weight 46.6 g/m²
29.1 lb/ream
ExxonMobil Method
ExxonMobil Bicor™ 52MBR666 OPP Film
Product Description: Bicor 52MBR666 is a biaxially oriented transparent polypropylene film coated with humidity resistant acrylic on both sides. This film is designed to wrap products with a high mo..