Physical Properties | Metric | English | Comments |
---|---|---|---|
Coating Weight | 26.6 g/m² | 16.6 lb/ream | ExxonMobil Method |
ExxonMobil Bicor® 30 ARW OPP Film Product Description: Bicor ARW is a two-side acrylic coated OPP film designed for use in lamination and monoweb applications, especially for paper ream wrap. The acrylic-coated side with the higher .. |