Physical Properties Metric English Comments
Coating Weight 26.6 g/m²
16.6 lb/ream
ExxonMobil Method
ExxonMobil Bicor® 30 ARW OPP Film
Product Description: Bicor ARW is a two-side acrylic coated OPP film designed for use in lamination and monoweb applications, especially for paper ream wrap. The acrylic-coated side with the higher ..