Polymer Property : Coating Weight = 1880 lb/ream Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Coating Weight 3000 g/m²

@Thickness 1.00 mm
1880 lb/ream

@Thickness 0.0394 in
Sharadaa Ceramics Heat Shield Zircon Rich Refractory Coating
Characteristics: Easy to mix with water – User friendly; Easy to apply by toweling, brushing or spraying; Adequate dry strength; Good adhesion to metals, refractory bricks and castables; No sur..