Sharadaa Ceramics Heat Shield Zircon Rich Refractory Coating

Category Ceramic , Oxide , Zirconium Oxide
Manufacturer Sharadaa Ceramics
Trade Name Heat Shield
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Sharadaa Ceramics Heat Shield Zircon Rich Refractory Coating.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Characteristics: Easy to mix with water – User friendly; Easy to apply by toweling, brushing or spraying; Adequate dry strength; Good adhesion to metals, refractory bricks and castables; No surface cracks or peel-off at operating temperatures; Increases life of refractory lining and heating systems; Odorless and non hazardousInformation provided by Sharadaa Ceramics Pvt. Ltd.
Physical Properties Metric English Comments
Coating Weight 3000 g/m²

@Thickness 1.00 mm
1880 lb/ream

@Thickness 0.0394 in
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 1550 °C
2820 °F
Continuous
1650 °C
3000 °F
Component Elements Properties Metric English Comments
Al2O3 2.54 %
2.54 %
CaO 1.5 %
1.5 %
SiO2 31.25 %
31.25 %
ZrO2 65.5 %
65.5 %
Descriptive Properties Value Comments
Color Cream
Thermal Shock Resistance Excellent