Physical Properties | Metric | English | Comments |
---|---|---|---|
Coating Weight | 18.4 g/m² | 11.5 lb/ream | ExxonMobil Method |
ExxonMobil Bicor™ 21MB866 OPP Film Product Description: Bicor 21MB866 is a high gas barrier, transparent biaxially oriented polypropylene film coated on side acrylic, one side PVOH. It provides excellent gas and aroma protection and .. |