Physical Properties | Metric | English | Comments |
---|---|---|---|
Coating Weight | 27.7 g/m² | 17.3 lb/ream | ExxonMobil Method |
ExxonMobil Bicor™ 30MB668 OPP Film Product Description: A high speed transparent, biaxially oriented polypropylene film, coated one side very low temperature seal (VLTS) coating. VLTS coating provides excellent performances on high s.. |
|||
Coating Weight | 27.7 g/m² | 17.3 lb/ream | ExxonMobil Method |
ExxonMobil Label-Lyte™ 30LL666 OPP Film Product Description: A transparent, high gloss, two side acrylic coated BOPP film for reel-fed wrap-around labeling applications.Availability: Africa & Middle East, Asia Pacific and EuropeKey Featur.. |
|||
Coating Weight | 27.7 g/m² | 17.3 lb/ream | ExxonMobil Method |
ExxonMobil Bicor™ 30MBT666 OPP Film Product Description: A biaxially oriented transparent polypropylene film, acrylic coated two sides. This film is specifically suitable for unsupported overwrapping, offering unique aspect and cost r.. |