Physical Properties Metric English Comments
Coating Weight 17.3 g/m²
10.8 lb/ream
ExxonMobil Method
ExxonMobil Bicor® 75 AB-X OPP Film
Product Description: Bicor AB-X is a two-side coated, sealable OPP film designed for general use in many applications, including overwrap, horizontal and vertical packaging. This film is suitable as..
Coating Weight 17.3 g/m²
10.8 lb/ream
ExxonMobil Method
ExxonMobil Label-Lyte™ 28LLG MET OPP Film
Product Description: A clear, one-side metallized, one-side treated oriented polypropylene film. The metalized layer is designed to provide a bright metal appearance in surface print or laminated ap..
Coating Weight 17.3 g/m²
10.8 lb/ream
ExxonMobil Method
ExxonMobil Label-Lyte™ 28LLG-202 OPP Film
Product Description: A white, two-side treated, polypropylene film designed for use in roll-fed labeling of cylindrical glass, plastic, and metal containers. Typical applications include food, bever..
Coating Weight 17.3 g/m²
10.8 lb/ream
0.5 m<sup>2</sup>; ASTM E252
DuPont Teijin Films Mylar® P25 Polyester Film, 50 Gauge
Product Description: Mylar® P25 is an uncoated, transparent polyester packaging film designed to be combined with a sealant layer, where the resulting structure will be shallow draw thermoformed. S..
Coating Weight 17.3 g/m²
10.8 lb/ream
0.5 m<sup>2</sup>; ASTM E252
DuPont Teijin Films Mylar® P25T Polyester Film, 50 Gauge
Product Description: Mylar® P25T is a transparent polyester packaging film designed to be combined with a sealant layer, where the resulting structure will be shallow draw thermoformed. It has a co..