Physical Properties | Metric | English | Comments |
---|---|---|---|
Drawdown | 9.17 m/s @Temperature 315 °C |
1810 ft/min @Temperature 599 °F |
Constant output at 35 rpm; ExxonMobil Method |
ExxonMobil LDPE LD 259 Low Density Polyethylene Resin (European Grade) Product Description: LD 259 is a LDPE extrusion coating grade, especially introduced for coating on non-woven substrates. Its high melt-index combines with low density gives this grade the right bal.. |