Physical Properties | Metric | English | Comments |
---|---|---|---|
Neck In | 12.7 cm | 5.00 in | at 280°C, 1.0 mil |
M. Holland Company MAGMA® LM233-A LLDPE
(discontinued **) Features: Good Heat Seal, Good ProcessabilityUses: Coating Applications, Film, Cast Film, PackagingProcessing Method: Coextrusion, Blown FilmInformation provided by M. Holland. |