Physical Properties Metric English Comments
Kinematic Viscosity 7400 cSt

@Temperature -40.0 °C
7400 cSt

@Temperature -40.0 °F
ASTM D445
ExxonMobil SpectraSyn Plus™ 6 Advanced Polyalphaolefin (PAO) Fluid
Product Description: SpectraSyn Plus™ Advanced Polyalphaolefin (PAO) provide an optimal combination of volatility and low-temperature fluidity. SpectraSyn Plus™ Advanced products viscosity indices..