ExxonMobil SpectraSyn Plus™ 6 Advanced Polyalphaolefin (PAO) Fluid

Category Fluid , Lubricant , Polyalphaolefin (PAO)
Manufacturer Exxon Chemical
Trade Name SpectraSyn Plus™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil SpectraSyn Plus™ 6 Advanced Polyalphaolefin (PAO) Fluid.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: SpectraSyn Plus™ Advanced Polyalphaolefin (PAO) provide an optimal combination of volatility and low-temperature fluidity. SpectraSyn Plus™ Advanced products viscosity indices translate into improved flow at low temperatures and increased film thickness at high temperatures. SpectraSyn Plus™ Advanced PAO provide superior lubrication as the primary basestocks for synthetic lubricants used in passenger car engines, heavy-duty diesel engines, transmissions, and a variety of industrial applications. SpectraSyn Plus™ Advanced PAO can be use for upgrading mineral oil or Group III basestock for improved low temperature and volatility performance. Appearance: Bright & ClearAvailability: Africa & Middle East, Asia Pacific, Central America, Europe, North America and South AmericaInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.827 g/cc

@Temperature 15.6 °C
0.0299 lb/in³

@Temperature 60.1 °F
ASTM D4052
Viscosity 1.86 cP
1.86 cP
High-Temp. High Shear; ASTM D5481
6243 cP

@Temperature -40.0 °C
6243 cP

@Temperature -40.0 °F
Apparent Viscosity by Mini-Rotary Viscometer; ASTM D4684
Brookfield Viscosity 6289 cP

@Temperature -40.0 °C
6289 cP

@Temperature -40.0 °F
ASTM D2983
Viscosity Measurement 143
143
Index; ASTM D2270
Kinematic Viscosity 7400 cSt

@Temperature -40.0 °C
7400 cSt

@Temperature -40.0 °F
ASTM D445
Kinematic Viscosity at 40°C (104°F) 30.3 cSt
30.3 cSt
ASTM D445
Kinematic Viscosity at 100°C (212°F) 5.9 cSt
5.9 cSt
ASTM D445
Vapor Pressure 0.000267 bar

@Temperature 150 °C
0.200 torr

@Temperature 302 °F
ASTM D2879
Evaporation Loss 5.7 %

@Temperature 205 °C,
Time 23400 sec
5.7 %

@Temperature 401 °F,
Time 6.50 hour
ASTM D972
Thermal Properties Metric English Comments
Pour Point <= -53.9 °C
<= -65.0 °F
ASTM D5950/D97
Flash Point 246 °C
475 °F
COC; ASTM D92
Optical Properties Metric English Comments
Refractive Index 1.4579
1.4579
ASTM D1218
Electrical Properties Metric English Comments
Dielectric Constant 2.11
2.11
ASTM D924
Dielectric Breakdown 39400 V
39400 V
Chemical Properties Metric English Comments
Acid Value <= 0.050
<= 0.050
[mg KOH/g]; ASTM D974 (mod)
Descriptive Properties Value Comments
Aniline Point 247°F
ASTM D611
Cold Cranking Simulator 1400 cP
-13°F, ASTM D5293
2247 cP
-22°F, ASTM D5293
3600 cP
-31°F, ASTM D5293
Color <0.5
ASTM D1500
Composition Water
<50 ppm, ASTM D6304 (mod)
Density Correction Factor 0.000632 (g/cc)/°C
ASTM D1250
Fire point 532°F
COC, ASTM D92
Noack Volatility <6%
ASTM D5800/DIN 51581