Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity | 55 cSt @Temperature 25.0 °C |
55 cSt @Temperature 77.0 °F |
ASTM D445 |
PolyOne Synplast™ DUP-E Di Undecyl Phthalate Linear C11 phthalate esterContains 0.10-0.15 wt% 1,1,3-Tris (2-methyl-4hydroxy-5-t-butyl phenyl) butane antioxidantInformation provided by PolyOne |
|||
Kinematic Viscosity | 55 cSt | 55 cSt | |
Dow Corning MOLYKOTE® BG-20 SYNTHETIC BEARING GREASE Polyol Ester grease especially for high speed bearingsFeatures: Lubricating bearings operating under a wide range of conditions, including high speeds, extreme temperatures and high loads. Handles .. |