Dow Corning MOLYKOTE® BG-20 SYNTHETIC BEARING GREASE

Category Fluid , Lubricant , Lithium Gellant
Manufacturer Dow Corning
Trade Name MOLYKOTE®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning MOLYKOTE® BG-20 SYNTHETIC BEARING GREASE.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Polyol Ester grease especially for high speed bearingsFeatures: Lubricating bearings operating under a wide range of conditions, including high speeds, extreme temperatures and high loads. Handles high speed, high load, high temperature combinations. Beige, lithium s thickened, polyolester grease. Applications: Lubricating electric motor bearings, bearings in fans, calendars, presses, generators, dryers, spindles, conveyors, index machines, switch contacts.Base Oil: EsterColor(s): BeigeThickener: Lithium complexNLGI#: 2Information provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 1.01 g/cc

@Temperature 25.0 °C
1.01 g/cc

@Temperature 77.0 °F
Kinematic Viscosity 55 cSt
55 cSt
Saybolt Viscosity at 100°F 200 SUS
200 SUS
Base Oil Viscosity
Mechanical Properties Metric English Comments
Four Ball Extreme Pressure, Weld Load 244.6 kg
539.3 lb (mass)
Penetration P(0), 1/10 mm 240 - 270
240 - 270
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 200 °C
392 °F
Minimum Service Temperature, Air -45.0 °C
-49.0 °F
Dropping Point >= 295 °C
>= 563 °F
Processing Properties Metric English Comments
Shelf Life 60.0 Month
60.0 Month
Descriptive Properties Value Comments
Color beige