Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity | 130 cSt | 130 cSt | |
Dow Corning FZ-2110 Dow Corning® FZ-2110 is a silicone polyether supplied at 100% solids that can be dispersed in water-based formulations and compatible with solvent-based formulations. This product demonstrates anti.. |