Dow Corning FZ-2110

Category Polymer , Thermoset , Silicone
Manufacturer Dow Corning
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning FZ-2110.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Dow Corning® FZ-2110 is a silicone polyether supplied at 100% solids that can be dispersed in water-based formulations and compatible with solvent-based formulations. This product demonstrates antifoam performance and, in water-based flexographic ink formulations, enhancement of film formation.Information provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 0.990 g/cc

@Temperature 25.0 °C
0.990 g/cc

@Temperature 77.0 °F
Solids Content 100 %
100 %
Kinematic Viscosity 130 cSt
130 cSt
Thermal Properties Metric English Comments
Flash Point 100 °C
212 °F
closed cup
Descriptive Properties Value Comments
Appearance clear