Polymer Property : Kinematic Viscosity = 12 cSt Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Kinematic Viscosity <= 12 cSt

@Temperature 49.9 - 50.1 °C
<= 12 cSt

@Temperature 122 - 122 °F
Kazanorgsintez K-8 Waste Diesel Fuel
Production Method: Waste diesel oil is produced when diesel oil is used a cracked gas cooling or flushing agent in the process of ethylene production. Application: Waste diesel oil is shipped to..
Kinematic Viscosity 12 cSt
12 cSt
3M Fluorinert™ FC-70 Electronic Liquid
Fluorinert™ Liquid FC-70 a non-conductive, thermally and chemically stable liquid that offers a high boiling point (215 deg C), it is ideal for many electronics single and two phase heat transfer a..