Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 9.74 - 9.94 g/cc | 0.352 - 0.359 lb/in³ | |
MarkeTech Cu/Mo/Cu 1:5:1 Laminated Sheet Cu/MoCu sheets have very high in-plane thermal conductivity provide by layers of Cu and low CTEs provided by the inner layer of molybdenum. These laminated sheets spread heat from a concentrated hea.. |